  • EC410NiMoAWS#2
  • AWS
EC410NiMo MH EC410NiMo
Specification: Tensile strength-ksi(MPa):110(760) Yield strength at 0.2% offset-ksi(Mpa):()Elongation(%):15 Hardness -HV(HRC):-(-) Preheat and Interpass: PWHT:Heat to 1100 to 1150°F(595 to 620°C), hold for one hour and air cool to ambient. -- Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.06 Si:0.9 Mn:1 P:0.04 S:0.03 Ni:5 Cr:12.5 Mo:0.7 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.75 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- …