Specification: Tensile strength-(ksi)Mpa:(100)690 Yield strength at 0.2% offset-(ksi)Mpa:(88)610 Elongation(%):16 Hardness -(HV)HRC:(-)- Preheat and Interpass:200°F~225°F(95°C~110°C) PWHT:1150°F ±25°F(620°C ±15°C) in 1 Hour IV-40°C(J):41 Type of Covering:- Shielding gas:Ar-20%Co2 Welding position:- Type of current:- C:0.08 Si:0.69 Mn:1.94 P:0.015 S:0.006 Cr:0.01 Ni:0.01 Mo:0.32 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.01 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/