Specification: Tensile strength-(ksi)Mpa:(110)760 Yield strength at 0.2% offset-(ksi)Mpa:() Elongation(%):15 Hardness -(HV)HRC:(-)- Preheat and Interpass: PWHT:Heat to 1100 to 1150°F(595 to 620°C), hold for one hour and air cool to ambient. IV °C(J):- Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.06 Si:0.9 Mn:1 P:0.04 S:0.03 Cr:12.5 Ni:5 Mo:0.7 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.75 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/