Specification: Tensile strength-(ksi)Mpa:(120)830 Yield strength at 0.2% offset-(ksi)Mpa:(108)740 Elongation(%):18 Hardness -(HV)HRC:(-)- Preheat and Interpass:200°F~250°F(95°C~120°C) PWHT:1075°F ±25°F(580°C ±15°C) in 1 Hour IV °C(J):- Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.1 Si:0.6 Mn:2.25 P:0.03 S:0.03 Cr:1.5 Ni:2.5 Mo:0.55 V:0.05 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.01 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/