Specification: Tensile strength-(ksi)Mpa:(100)690 Yield strength at 0.2% offset-(ksi)Mpa:(88)610 Elongation(%):16 Hardness -(HV)HRC:(-)- Preheat and Interpass:325°F~375°F(160°C~190°C) PWHT:1275°F ±25°F(690°C ±15°C) in 1 Hour IV-18°C(J):27min. Type of Covering:- Shielding gas:100%Co2 Welding position:- Type of current:- C:0.12 Si:0.57 Mn:1.55 P:0.03 S:0.03 Cr:0.28 Ni:1.5 Mo:0.47 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.35 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/