Specification: Tensile strength-(ksi)Mpa:(100)690 Yield strength at 0.2% offset-(ksi)Mpa:(88)610 Elongation(%):16min. Hardness -(HV)HRC:(-)- Preheat and Interpass:200°F~225°F(95°C~110°C) PWHT:1150°F ±25°F(620°C ±15°C) in 1 Hour IV-12°C(J):256 Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.15 Si:0.5 Mn:1.45 P:0.02max S:0.02max Cr:0.3 Ni:1.75 Mo:0.55 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.35 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/