Specification: Tensile strength-(ksi)Mpa:(100)690 Yield strength at 0.2% offset-(ksi)Mpa:(88)610 Elongation(%):16 Hardness -(HV)HRC:(-)- Preheat and Interpass:200°F~250°F(95°C~110°C) PWHT:1075°F ±25°F(580°C ±15°C) in 1 Hour IV-40°C(J):27min. Type of Covering:Low hydrogen postassium Shielding gas:- Welding position:F, V, OH, H Type of current:AC or DCEP C:0.07 Si:0.6 Mn:1.4 P:0.03 S:0.03 Cr:0.4 Ni:3.8 Mo:0.6 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.01 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/