Specification: Tensile strength-(ksi)Mpa:(110)760 Yield strength at 0.2% offset-(ksi)Mpa:(90)620 Elongation(%):15 Hardness -(HV)HRC:(-)- Preheat and Interpass:Heat to 210 to 390°F(100 to 200°C) PWHT:Heat to 1100 to 1150°F(595 to 620°C), hold for one hour and air cool to ambient. IV °C(J):- Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.03 Si:0.25 Mn:0.8 P:0.01 S:0.01 Cr:12 Ni:4.5 Mo:0.6 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.05 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/