Specification: Tensile strength-(ksi)Mpa:(70)480 Yield strength at 0.2% offset-(ksi)Mpa:(58)400 Elongation(%):22min. Hardness -(HV)HRC:(-)- Preheat and Interpass:- PWHT:- IV °C(J):- Type of Covering:Low-hydrogen postassium, iron powder Shielding gas:- Welding position:H-Fillet Type of current:AC or DCEP C:0.07 Si:0.29 Mn:1.08 P:0.027 S:0.015 Cr:0.01 Ni:0.01 Mo:0.01 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.01 Ti:- B:- Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/