Specification: Tensile strength-(ksi)Mpa:(70)480 Yield strength at 0.2% offset-(ksi)Mpa:(58)400 Elongation(%):22min. Hardness -(HV)HRC:(-)- Preheat and Interpass:- PWHT:- IV °C(J):- Type of Covering:- Shielding gas:- Welding position:- Type of current:- C:0.05 Si:0.82 Mn:1.53 P:0.013 S:0.01 Cr:0.01 Ni:0.01 Mo:0.01 V:0.01 W:0.01 Nb(Cb)+Ta:0.01 N:- Cu:0.21 Ti:0.18 B:0.006 Co:- Fe:Rem Al:0.01 Zn:- Ca:- Mg:- Fn:- Sn:- Other:… ...see more… Liên hệ 0982 010609, Website:http://aladins.vn/